I racked and stabilised some WoW 2-3 weeks ago, without using any finings. They have half cleared, in that you can see through them, but they are still on the cloudy side. They've been clearing at around 17-20C, which could be slowing the process down, but I don't want to put them in the shed where it is likely too cold (-3 to +5C currently)
I'm going to pick up some finings or kwikclear this weekend, providing the weather allows me to get to my LHBS, as I'd like to bottle them soon as I need the DJs for my next batch!